Nickel 200
Features:
UNS Number N02200


Nickel 200 is developed by 96% commerce. It has a high reducing chemicals resistance. Nickel 200 can also be used in the oxidizing conditions which could cause the formation of a passive oxide film. Nickel 200 is limited to service at the temperatures below 315℃ to avoid suffering from graphitization that can results in severely compromised properties. In that circumstance, Nickel 201 is used instead. It has a high curie temperature and good magnetostrictive properties. Its thermal and electrical conductivities are higher than nickel alloys.

Applications:
The applications of Nickel 200 is used in the area where maintains product purity such as handling of caustic alkalis, foods and synthetic fibers; electrical and electronic parts; aerospace and missile components; and chemical storage and shipping tanks.

Products of Nickel 200 available
• Sheet
• Plate
• Bar
• Pipe & Tube (welded & seamless)
• Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)

• Wire


Chemical composition:

% Ni Fe C Mn Si S Cu
min 99.0
max 0.40 0.15 0.35 0.35 0.010 0.25

Physical properties:
Density 8.89 g/cm3
Melting range 1435-1446℃

ASTM Specifications
Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet/Plate Bar Fitting
B161 B622 B161 B622 B162 B160 B163