Features:
Rene41 is a precipitation hardening deformed high temperature and high strength alloy.
It has high tensile and durable creep strength and good oxidation resistance in the range of 650-900℃.
Applications:
It is suitable for manufacturing high-temperature parts of aviation and aerospace engines with high strength and oxidation resistance below 870 ° C and 980 ° C.
Physical properties:
|
Density |
8.27 g/cm³ |
|
Melting Point |
1316-1371 ℃ |
Nominal composition,%
|
Alloy designation |
Ni |
Cr |
Co |
Mo |
W |
Ta |
Nb |
Al |
Ti |
Fe |
Mn |
Si |
C |
B |
Zr |
|
Rene41 |
55 |
19 |
11 |
10 |
|
|
|
1.5 |
3.1 |
|
|
|
0.09 |
0.005 |
|