Alloy 31
Alloy 31 is an iron-nickel-chromium-molybdenum alloy with nitrogen addition. It has a pitting resistance in high chloride environments between those of super-austenitic stainless steels and nickel alloys. The alloy has very good corrosion resistance in mixed acid and high chloride environments. The material is approved in ISO 15156/ NACE MR0175 to test level VI for sour gas service.
Alloy 31 Mechanical Properties:
Temper | Annealed | |
---|---|---|
Tensile Rm | 94 | ksi (min) |
Tensile Rm | 650 | MPa (min) |
R.p. 0.2% Yield | 41 | ksi (min) |
R.p. 0.2% Yield | 280 | MPa (min) |
Elongation (2.02 or 4D gl) | 40 | % (min) |
Element | Min | Max |
---|---|---|
C | - | 0.0015 |
Si | - | 0.3 |
Mn | - | 2 |
P | - | 0.02 |
S | - | 0.01 |
Cr | 26 | 28 |
Cu | 1 | 1.4 |
Fe | Balance | |
Mo | 6 | 7 |
N | 0.15 | 0.25 |
Ni | 30 | 32 |