Features:
UNS Number N08810
Incoloy 800H has a restricted carbon content range of 0.05 to 0.10%, which is in the upper portion of that of Incoloy 800, and is annealed at 1149 to 1177℃ (Incoloy 800 is annealed at 983 to 1038℃). These differences impart it to have higher stress rupture and creep properties than Incoloy 800.
Applications:
Chemical and petrochemical process piping, high temperature heat exchangers, furnace components, carburizing equipment, heating-element sheathing, and nuclear power steam superheating tubing.
Products of Incoloy 800H available
• Sheet
• Plate
• Bar
• Pipe & Tube (welded & seamless)
• Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
• Wire
Chemical composition:
|
%
|
Fe
|
Ni
|
Cr
|
C
|
Mn
|
Si
|
S
|
Cu
|
Al
|
Ti
|
|
Min
|
39.5
|
30.0
|
19.0
|
0.05
|
|
|
|
|
0.15
|
0.15
|
|
Max
|
|
35.0
|
23.0
|
0.10
|
1.50
|
1.00
|
0.015
|
0.75
|
0.60
|
0.60
|
Physical properties:
|
Density
|
7.94 g/cm3
|
|
Melting range
|
1357-1385℃
|
ASTM Specifications
|
Alloy
|
Pipe Smls
|
Pipe Welded
|
Tube Smls
|
Tube Welded
|
Sheet/Plate
|
Bar
|
Forging
|
Fitting
|
|
Alloy 800 (UNS N08800)
|
B407
|
B154
|
B163
|
B515
|
B409
|
B408
|
B564
|
B366
|
|
Alloy 800H (UNS N08810)
|
B407
|
B154
|
B163
|
B515
|
B409
|
B408
|
B564
|
B366
|
|
Alloy 800HT (UNS N08811)
|
B407
|
B154
|
B163
|
B515
|
B409
|
B408
|
B564
|
B366
|