Chemical composition
|
Grade |
C |
Si |
Mn |
P |
S |
Ni |
Cr |
Mo |
|
301 |
≤0 .15 |
≤l.0 |
≤2.0 |
≤0.045 |
≤ 0.03 |
6.0-8.0 |
16.0-18.0 |
- |
|
302 |
≤0 .15 |
≤1.0 |
≤2.0 |
≤0.035 |
≤ 0.03 |
8.0-10.0 |
17.0-19.0 |
- |
|
304 |
≤0 .0.08 |
≤1.0 |
≤2.0 |
≤0.045 |
≤ 0.03 |
8.0-10.5 |
18.0-20.0 |
- |
|
304L |
≤0.03 |
≤1.0 |
≤2.0 |
≤0.035 |
≤ 0.03 |
9.0-13.0 |
18.0-20.0 |
- |
|
309S |
≤0.08 |
≤1.0 |
≤2.0 |
≤0.045 |
≤ 0.03 |
12.0-15.0 |
22.0-24.0 |
- |
|
310S |
≤0.08 |
≤1.5 |
≤2.0 |
≤0.035 |
≤ 0.03 |
19.0-22.0 |
24.0-26.0 |
|
|
316 |
≤0.08 |
≤1.0 |
≤2.0 |
≤0.045 |
≤ 0.03 |
10.0-14.0 |
16.0-18.0 |
2.0- |
|
3 |
||||||||
|
316L |
≤0 .03 |
≤1.0 |
≤2.0 |
≤0.045 |
≤ 0.03 |
12.0 - 15.0 |
16 .0 -1 8.0 |
2.0 - |
|
3 |
||||||||
|
321 |
≤ 0 .08 |
≤1.0 |
≤2.0 |
≤0.035 |
≤ 0.03 |
9.0 - 13 .0 |
17.0 -1 9.0 |
- |
|
630 |
≤ 0 .07 |
≤1.0 |
≤1.0 |
≤0.035 |
≤ 0.03 |
3.0-5.0 |
15.5-17.5 |
- |
|
631 |
≤0.09 |
≤1.0 |
≤1.0 |
≤0.030 |
≤0.035 |
6.50-7.75 |
16.0-18.0 |
- |
|
904L |
≤ 2 .0 |
≤0.045 |
≤1.0 |
≤0.035 |
- |
23.0·28.0 |
19.0-23.0 |
4.0-5.0 |
|
2205 |
≤0.03 |
≤1.0 |
≤2.0 |
≤0.030 |
≤0.02 |
4.5-6.5 |
22.0-23.0 |
3.0-3.5 |
|
2507 |
≤0.03 |
≤0.8 |
≤1.2 |
≤0.035 |
≤0.02 |
6.0-8.0 |
24.0-26.0 |
3.0-5.0 |
|
2520 |
≤0.08 |
≤1.5 |
≤2.0 |
≤0.045 |
≤ 0.03 |
0.19 -0. 22 |
0. 24 -0 . 26 |
- |
|
410 |
≤0.15 |
≤1.0 |
≤1.0 |
≤0.035 |
≤ 0.03 |
- |
11.5-13.5 |
- |
|
430 |
≤0.1 2 |
≤0.75 |
≤1.0 |
≤ 0.040 |
≤ 0.03 |
≤0.60 |
16.0 -18.0 |
- |