In792-SX Chemical composition:
Nominal composition,%
|
Alloy designation |
C |
Ni |
Cr |
Co |
Mo |
Fe |
Al |
B |
Ti |
W |
Nb |
Zr |
V |
|
IN792-SX |
0.2 |
60 |
13 |
9 |
2.0 |
|
3.2 |
0.02 |
4.2 |
4 |
2 |
0.1 |
|