Alloy 52
Nominal composition,%
|
Alloy designation |
Ni |
Cr |
Mn |
Si |
C |
Al |
Mn |
P |
S |
Fe |
|
Alloy 52 |
50.5 |
0.25 max |
0.80 max |
0.30 max |
0.05 max |
0.10 max |
0.5max |
0.025 max |
0.025 max |
Bal |