Hastelloy B-2
Description: Hastelloy B-2 / N10665 / NS322 / 2.4617
Features: Hastelloy B-2 has outstanding resistance to hydrochloric acid at all concentrations and temperatures. It also has significant resistance to reducing environments like sulfuric, phosphoric, acetic acids and other nonoxidizing media. Hastelloy B-2 has excellent resistance to pitting corrosion, stress corrosion cracking, and knife line and weld heat-affected zone attack. Hastelloy B-2 has poor resistance to oxidizing environments, therefore, it should not be used where ferric or cupric salts are present as these salts may cause rapid corrosion failure.
Applications: Equipment handling reducing chemical environments; and chemical process industry involving hydrochloric, sulfuric, phosphoric and acetic acids.
Hastelloy B Chemical compostion:
| Alloy | % | Ni | Mo | Fe | Cr | Co | C | Mn | V | Si | P | S |
| Hastelloy B | Min. | Balance | 26 | 4 | 0.2 | |||||||
| Max. | 30 | 6 | 1 | 2.5 | 0.05 | 1 | 0.4 | 1 | 0.04 | 0.03 | ||
| Hastelloy B-2 | Min. | Balance | 26 | 2 | ||||||||
| Max. | 30 | 7 | 1 | 1 | 0.02 | 1 | 0.1 | 0.04 | 0.03 |
Hastelloy B Physical properties:
| Density | 9.24g/cm3 |
| Melting point | 1330-1380℃ |
Hastelloy B Alloy minimum mechanical properties in the room temperature:
| Alloy state | Tensile strength | Yield strength | Elongation |
| Rm N/mm2 | RP0.2N/mm2 | A5 % | |
| Hastelloy B | 690 | 310 |
40 |