S6 Material grades and equivalents: Stellite 6; UNS R30006; AMS 5387C-2001
Introduction:
Stellite 6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.
Stellite Chemical components
C |
Cr |
Si |
W |
Fe |
Mo |
Ni |
Mn |
B |
Co |
1.2 |
28 |
1.1 |
4.5 |
3 |
|
3 |
1 |
|
bal |
*The chemical composition shown above is an outline only,and should not be taken as a full specification. |
Density |
Specific |
Solidus |
Liquidus |
Specific heat |
Magnetic |
Electrode |
Electrical |
Electrical |
0.305 |
8.46 |
2340°F |
2540°F |
0.101°F |
<1.2@200 |
-0.25 |
1.9%IACS |
41.73 |
Regular shape for all kinds of alloys |
|||
Form |
Specification |
Supply Form |
Others |
Sheet |
Thickness:0.40-4.75mm,General Width:1000、1219、1500mm |
Whole Coil or piece of it |
Cold Annealed,Surface 2B、2E |
Plate |
Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) |
Whole Coil or piece of it |
Single hot rolling,Solid solution annealed state,Surface 1D |
Belt |
Thickness:0.10-3.0mm,Width:50-500mm |
Whole Coil or Specified size |
Cold Annealed,Surface 2B、2E |
Bar & Rod |
Rolled barΦ5-45mm,Length≤1500mm |
Polished Bar(circle、Square) |
Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm |
|||
Weld tube |
Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm |
Base on your requirement |
|
Seamless Tube |
Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm |
Base on your requirement |
|
Wire |
Outer diameterΦ0.1-13mm |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
Forged piece |
discs,rings,squares,blocks,slabs |
Base on your requirement |
Steel, Alloy |
Flangs |
All kinds of Flangs |
Base on your requirement |
Steel, Alloy |
Welding Material |
Coil wire Φ0.025mm-1.6mm |
Base on your requirement |
Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm |
|||
Welding rodΦ1.2mm-4.0mm |
|||
Tube |
Elbow, three links, four links, different diameter size |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate |
Raw Sheet Thickness≥2mm |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |