Refractaloy 26

R26 Material grades and equivalents

R26/GB GH26/UNS Refractaloy-26/SEW VDIUV W. Nr.1.2888

R26/GB GH26/UNS Refractaloy-26/SEW VDIUV W. Nr.1.2888 has excellent resistance to relaxation, anti creep property, permanence property and resistance to stress corrosion resistance.

HY R26 Chemical composition

Alloy

%

Ni

Cr

Fe

Mo

Ti

Co

R26

Min

Rest

Max

37

18

3

2.7

20



HY R26 Characteristic

HY R26 has excellent resistance to relaxation, anti creep property, permanence property and resistance to stress corrosion resistance.

Physical properties:

Density:9.14 g/cm3

Melting point:1300℃-1330 ℃


Alloy sheet mechanical properties in the room temperature:

Alloy Status

Tensile strength
Rm N/mm²

Yield strengthRP0.2 N/mm²

Elongation
A5 %

Solution Treatment

925

610

10



HY R26 Application field

HY R26 is a material can be applied in turbine engine blade and fastener.



Regular shape for all kinds of alloys

Form

Specification

Supply Form

Others

Sheet

Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

Whole Coil or piece of it

Cold Annealed,Surface 2B、2E

Plate

Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

Whole Coil or piece of it

Single hot rolling,Solid solution annealed state,Surface 1D

Belt

Thickness:0.10-3.0mm,Width:50-500mm

Whole Coil or Specified size

Cold Annealed,Surface 2B、2E

Bar & Rod

Rolled barΦ5-45mm,Length≤1500mm

Polished Bar(circle、Square)

Solution annealing,descaling

Forged barΦ26-245mm,Length≤4000mm

Weld tube

Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

Base on your requirement

Seamless Tube

Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

Base on your requirement

Wire

Outer diameterΦ0.1-13mm

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy

Forged piece

discs,rings,squares,blocks,slabs

Base on your requirement

Steel, Alloy

Flangs

All kinds of Flangs

Base on your requirement

Steel, Alloy

Welding Material

Coil wire Φ0.025mm-1.6mm

Base on your requirement

Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

Straight WireΦ1.6mm-4.0mm

Welding rodΦ1.2mm-4.0mm

Tube

Elbow, three links, four links, different diameter size

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy

Explosive bonded laminate

Raw Sheet Thickness≥2mm

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy




Product Catalog