Alloy |
% |
Ni |
Cr |
Fe |
Co |
Cu |
C |
Mn |
Si |
P |
S |
Mo |
4J29 |
Min |
28.5 |
|
Balance |
16.8 |
|
|
|
|
|
|
|
Max. |
29.5 |
0.2 |
17.8 |
0.2 |
0.03 |
0.5 |
0.3 |
0.02 |
0.02 |
0.2 |
The expansion coefficient of 4J29 alloy in a wide temperature range (-80-450℃) is similar to that of hard glass. In the electric vacuum industry, it is used to seal hard glass to make high-airtight components. It can also be used with hard glass. Ceramic sealing. Name: Fe-Ni-Co glass sealing alloy. At 20~450 ℃, it has a thermal expansion coefficient similar to that of borosilicate hard glass, a high Curie point, and good low-temperature structural stability. It is an iron-nickel-cobalt glass sealing alloy.