Features:

NIMONIC alloy 115 (W. Nr. 2.4636) is a nickelchromium-cobalt based alloy, strengthened with additions of molybdenum, aluminum and titanium. 


Application:

It was developed as a creep-resisting alloy for service at temperatures up to about 1010°C, as turbine blades for aircraft gas turbines, which is available for supply in bar form and extruded sections.   The material is known as a creep-resisting alloy and with initial development for high-temperature service operation up to 1010°C

. 


Nominal composition,%

Alloy 

designation

C

Ni

Cr

Co

Mo

Fe

Al

B

Ti

W

Ta

Zr

V

Nimonic115

0.15

60

14.3

13.2

3.3

-

4.9

0.16

3.7

-

-

0.04

-