Nitronic 50 is used in such applications as seawater pumps, gate valves for seawater ballast systems on tankers, high-pressure (microbial) deep-sea sampler and incubation chambers and underwater robotic arms, urea production, ammonium carbamate pumps, pressure vessels, tanks, heat exchangers, piping, fittings, valves and pumps, oil field production and down-hole equipments.
Nitronic 50 Chemical Composition:
| Grade | Ni% | Cr% | Fe% | C% | Mn% | Si% | N% | Mo% | Nb% | V% | P% | S% |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Nitronic 50 | 11.5-13.5 | 20.5-23.5 | 52-62 | Max 0.06 | 4.0-6.0 | Max 1.0 | 0.2-0.4 | 1.5-3.0 | 0.1-0.3 | 0.1-0.3 | Max 0.04 | Max 0.03 |
| Grade | Density | Melting Point |
|---|---|---|
| Nitronic 50 | 7.8 g/cm3 | 1415 °C-1450 °C |
|
Condition |
Tensile Strength |
Yield Strength σp0.2/MPa |
Elongation |
Reduction% |
|
Solution Treated |
Min 690 Mpa |
Min 380 Mpa |
Min 35% |
Min 55% |